Interfacial activation and mechanical contouring stabilize anodeless and solid-state cycling at low temperature and high rate without bulk material changes.
Anodeless all-solid-state pouch cells lose capacity at 5 °C when Li-Ag alloying stays kinetically suppressed, producing extrusion and delamination at the interlayer [1]. A single elevated-temperature formation cycle creates a stable alloy network that thereafter supports continued transport at sub-ambient conditions. This processing step converts a temperature-dependent kinetic barrier into a permanent pathway, showing that operational limits can be addressed through protocol rather than new bulk synthesis.
The same principle of enlarging effective contact area appears in contoured Li/Li6PS5Cl interfaces, where an egg-box topography raises the current density at which voiding begins by an order of magnitude [2]. Both approaches therefore operate on existing cell formats and shift failure thresholds without requiring changes to electrolyte composition or electrode loading. The tension lies in whether these activation or contouring steps remain effective once the cells encounter the full range of rates, temperatures and stack pressures encountered in field use.
If either route proves transferable, sub-ambient and high-rate operation of anodeless cells could advance without waiting for next-generation electrolytes [1, 2]. The result also reframes formation as an active design variable rather than a fixed manufacturing step.
The essentials
Low-temperature activation of Ag-C interlayers. Anodeless all-solid-state pouch cells with Ag-C interlayers exhibit temperature-dependent Li-Ag alloying that is rapid at 45 °C but kinetically limited at 5 °C, causing extrusion and delamination [1]. A single 45 °C formation cycle creates a stable alloy network that thereafter permits 87 % capacity retention after 250 cycles at 5 °C and roughly triple the discharge capacity of fixed-temperature cells [1]. Whether the alloy network remains stable under extended high-rate pulsing at 5 °C remains unresolved.
Al/F co-doped argyrodite for organic cathodes. Dual-site substitution in Li5.7Al0.1P0.9S4.5Cl1.2F0.3 raises ligand basicity, reduces anthracenetetrone adsorption energy from -4.41 to -0.15 eV and suppresses interfacial redox reactions while preserving 3.8 mS cm-1 conductivity [3]. Lithium plating/stripping exceeds 3000 h and ATO-based cells retain 81 % capacity after 2000 cycles at 5 C and 60 °C [3]. The abstract does not specify whether the same electrolyte stabilizes other high-voltage organic structures.
Colloid additives for anode-free sodium cells. Two-dimensional AgS nanosheets bearing fluorinated groups decompose at the sodium-electrolyte interface to produce a graded NaF/Na2S SEI that enables dendrite-free plating [4]. High-loading anode-free cells exceed 1600 cycles and 0.5 Ah pouch cells reach 500 cycles at 2 C [4]. Whether the graded SEI composition changes with prolonged cycling at 2 C remains unresolved.
Contoured interfaces against discharge voiding. An egg-box topography at the Li/Li6PS5Cl boundary increases the voiding onset current density tenfold from 0.2 to 2 mA cm-2 at 2 MPa and 30 °C while sustaining pulsed currents up to 3 mA cm-2 at 30 °C [2]. The contoured interface also passes Worldwide Harmonized Light Vehicles Test Procedure discharge profiles that cause rapid failure in flat interfaces [2]. The abstract does not specify long-term cycling retention under the same conditions.
Weakly coordinating fluoromethane electrolytes. A perfluorinated alkoxyaluminate salt in liquefied fluoromethane simultaneously weakens Li-solvent and Li-anion interactions, yielding 39.2 mS cm-1 conductivity and a lithium transference number of 0.71 in preprint measurements [5]. Nickel-rich cathode/lithium-metal cells charge at 10 C at room temperature and 2 C at -40 °C [5]. How the transference number evolves during extended cycling at -40 °C remains unresolved.
Mechanism and evidence
The clearest mechanistic advance lies in the temperature-gated Li-Ag alloying observed by operando X-ray absorption spectroscopy and cryogenic microscopy, which directly links suppressed alloy formation to extrusion and delamination [1]. The single-cycle activation protocol converts this kinetic barrier into a permanent transport pathway, an outcome replicated across multiple pouch cells. Parallel evidence from contoured Li6PS5Cl interfaces shows that geometric enlargement of contact area delays void nucleation by an order of magnitude under realistic stack pressure [2]. Both findings rest on cell-level testing rather than material-level proxies and therefore carry direct implications for formation protocols and interface topography. The preprint on weakly coordinating anions further demonstrates that simultaneous reduction of solvent and anion binding can relax the conductivity-transference trade-off, providing a third route to improved low-temperature kinetics [5].
Materials and interfaces
Al/F substitution in argyrodite electrolytes alters local bonding to reduce carbonyl adsorption energy and thereby passivates the cathode-electrolyte boundary while maintaining high ionic conductivity [3]. In sodium systems, in-situ decomposition of fluorinated nanosheets generates a functionally graded SEI whose spatial distribution of NaF and Na2S species appears responsible for sustained dendrite suppression [4]. Preprint measurements on weakly coordinating anions demonstrate that simultaneous reduction of solvent and anion binding relaxes the usual conductivity-transference trade-off [5]. These interface modifications operate through distinct chemical or geometric levers, suggesting a potential for extended cycling without bulk electrolyte redesign.
Scale-up, safety and manufacturing
The activation protocol for Ag-C interlayers and the egg-box contouring of Li6PS5Cl both operate on existing cell formats and therefore avoid new material synthesis routes [1, 2]. The 0.5 Ah anode-free sodium pouch cells cycled for 500 cycles at 2 C further indicate that colloid-derived SEIs can be integrated into practical cell assembly without additional formation hardware [4]. These processing steps address contact and transport limits at the electrode scale rather than at the gigafactory level. The absence of reported stack-pressure values in several studies leaves open how the observed gains translate once cells are built to lean-electrolyte targets typical of commercial formats.
Quick Radar
- Cryo-APT edge access: An upright-mounting workflow enables site-specific preparation of electrolyte-wetted graphite edges and perimeter Li dendrites for atom-probe tomography [6].
- NiBi reconstruction control: Weakly exothermic NiBi intermetallics limit Bi ligament coarsening to 65.3 nm average size and deliver 93.1 % retention after 20 000 cycles in sodium-ion cells [7].
- Additive incompatibility mechanism: KAIST measurements show that certain electrolyte-additive pairs prevent protective interphase formation and accelerate capacity loss [8].
- Semi-solid-state UPS cells: Ampace PU100 systems passed large-scale UL 9540A fire testing while supporting high-rate discharge required for data-center backup [9].
- Medium-entropy NASICON stability: Homogeneous Na3.0V0.5Mn0.5Ti0.5Cr0.5(PO4)3 exhibits 91 % retention after 5000 cycles at 2 A g-1 with 5.3 % volume change [10].
- MARS health-prediction framework: A multi-scale encoder plus constrained Kalman filter achieves mean absolute SOH errors of 0.72 % on NASA and CALCE datasets [11].
Closing
Whether the single-cycle thermal activation demonstrated for Ag-C interlayers can be translated to other anodeless chemistries without introducing new side reactions remains the immediate experimental question [1].
Sources
- Nature Communications: Low-temperature operation of Ag - C based anodeless all-solid-state pouch cells - https://www.nature.com/articles/s41467-026-79291-1
- Nature Energy: Contouring mitigates voiding at the lithium/ceramic electrolyte interface on discharging solid-state batteries - https://www.nature.com/articles/s41560-026-02172-w
- Advanced Energy Materials: Al/F Co-Doped Sulfide Electrolyte for Durable All-Solid-State Lithium-Organic Batteries - https://advanced.onlinelibrary.wiley.com/doi/10.1002/aenm.71853
- Journal of the American Chemical Society: Taming Metal-Electrolyte Interface via Two-Dimensional Organic Metal Chalcogenide Colloids for Anode-Free Sodium Metal Batteries - https://pubs.acs.org/jacsat/article-abstract/doi/10.1021/jacs.6c21804/5473871/Taming-Metal-Electrolyte-Interface-via-Two
- arXiv preprint: Weakly coordinating anions and solvents break the conductivity-transference-solvation tradeoff - https://arxiv.org/abs/2611.25375v1
- arXiv preprint: Accessing Electrode Edges: Upright Mounting for Site-Specific Cryogenic Atom Probe Tomography of Lithium-Ion Batteries - https://arxiv.org/abs/2611.21357v1
- ACS Nano: Weakly Exothermic Intermetallic NiBi Anode Enables Ultrafine Reconstruction for High-Rate Sodium-Ion Storage - https://pubs.acs.org/ancac3/article-abstract/doi/10.1021/acsnano.6c16600/5473861/Weakly-Exothermic-Intermetallic-NiBi-Anode-Enables
- Tech Xplore: Why combining battery additives can shorten battery life - scientists propose an alternative - https://techxplore.com/news/2026-11-combining-battery-additives-shorten-life.html
- Batteries News: Ampace Highlights AIDC Battery Safety and Semi-Solid-State Technology for AI Data Centres - https://batteriesnews.com/ampace-highlights-aidc-battery-safety-and-semi-solid-state-technology-for-ai-data-centres/
- Journal of Energy Chemistry: Enabling fast and reversible kinetics via TM-O bond modulation in homogeneous solid-solution medium-entropy NASICON for sodium ion batteries - https://www.sciencedirect.com/science/article/pii/S2095495626006145
- arXiv preprint: MARS: Feature-guided physics-informed deep learning for real-time battery health and lifetime prediction - https://arxiv.org/abs/2611.22455v1